Romania STAS/SR OLC15 Structural steel and OLC15 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | OLC15 | STAS/SR | Romania | Structural steel | 
| OL50.1 | |||||
| OL52.2 | |||||
| OL2.3 | |||||
| OL52.4 | |||||
| OL60.1 | |||||
| OL70.1 | |||||
| OLC10 | |||||
| OLC10S | |||||
| OLC10X | |||||
| OLC10XS | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 611 (≥) | 773 (≥) | 31 | 11 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 413 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.14 | - | |||
| 288 | 131 | - | 41.3 | 123 | - | ||
| 796 | - | 43 | 14.2 | 211 | 243 | 
Heat treated : 1229°C - 1123°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| OLC15 | STAS/SR | Romania | Structural steel | 
| OLC15S | STAS/SR | Romania | Structural steel | 
| OLC15X | STAS/SR | Romania | Structural steel | 
| OLC15XS | STAS/SR | Romania | Structural steel | 
| OLC15q | STAS/SR | Romania | Alloy structural steel | 
| OLC15q | STAS/SR | Romania | Alloy structural steel | 
| OLC15AT | STAS/SR | Romania | Alloy structural steel | 