Euronorm EN EN X3CrNiMo13-41 Euronorm Stainless Steel and EN X3CrNiMo13-41 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X3CrNiMo13-41 | EN | Euronorm | Euronorm Stainless Steel | 
| EN X2CrNiMo18-14-3 | |||||
| EN X2CrNiMoCuN25-6-3 | |||||
| EN X2CrNiMoCoWN25-7-4 | |||||
| EN X2CrNiMoN17-11-2 | |||||
| EN X2CrNiMoN17-13-3 | |||||
| EN X2CrNiMoN22-5-3 | |||||
| EN X2CrNiMoN25-7-4 | |||||
| EN X2CrMNi8-10 | |||||
| EN X2CrNiN23-4 | |||||
| EN X30Cr13 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | 
|---|---|---|---|---|---|---|---|
| 0.05 | 0.70 | 1.50 | 0.040 | 0.015 | 12.0-14.0 | 3.50-4.50 | 0.30-0.70 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 424 (≥) | 622 (≥) | 42 | 34 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 42 | - | - | 0.13 | - | |||
| 412 | 681 | - | 21.3 | 333 | - | ||
| 123 | - | 31 | 34.2 | 123 | 131 | 
Heat treated : 1935°C - 1351°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X3CrNiMo13-41 | EN | Euronorm | Euronorm Stainless Steel | 