E26-4
France AFNOR AIR 9160 C E26-4 AIR 9160 E26-4 and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
France AFNOR AIR 9160 C E26-4 AIR 9160 E26-4 and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | E26-4 | AFNOR | France | AIR 9160 E26-4 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
857 (≥) | 782 (≥) | 14 | 43 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.11 | - | |||
182 | 636 | - | 42.3 | 324 | - | ||
235 | - | 13 | 21.2 | 224 | 112 |
Grade | Standard | Country | Application |
---|---|---|---|
E26-4 | AFNOR | France |
AIR 9160 E26-4
|
Standard No. | Description | Download |
---|---|---|
AIR 9160 C |