Germany DIN 1.2345 Hot working alloy tool steel and 1.2345 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | 1.2345 | DIN | Germany | Hot working alloy tool steel | 
| 1.2313 | |||||
| 48CrMoV6-7 | |||||
| 1.2323 | |||||
| X35CrMoV5-1-1 | |||||
| 1.2324 | |||||
| X38CrMoV5-1 | |||||
| 1.2343 | |||||
| X40CrMoV5-1 | |||||
| 1.2344 | |||||
| X50CrMoV5-1 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | 
|---|---|---|---|---|---|---|---|
| 0.48-0.53 | 0.80-1.10 | 0.20-0.40 | Max 0.030 | Max 0.030 | 4.80-5.20 | 1.25-1.45 | 0.80-1.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 947 (≥) | 686 (≥) | 12 | 13 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.22 | - | |||
| 696 | 786 | - | 11.3 | 132 | - | ||
| 735 | - | 42 | 13.2 | 121 | 242 | 
Heat treated : 1619°C - 1316°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...