France AFNOR Z12CN18-09 Stainless Steel Plate & Steel Strip and Z12CN18-09 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z12CN18-09 | AFNOR | France | Stainless Steel Plate & Steel Strip | 
| Z8CN17 | |||||
| Z8CN25-20 | |||||
| Z8CNT12 | |||||
| Z9CNA17-07 | |||||
| Z10CNDA15-07 | |||||
| Z10NC32-21 | |||||
| Z11CN17-08 | |||||
| Z11CN18-08 | |||||
| Z11CNS17-07Az | |||||
| Z12CMN17-07Az | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | 
|---|---|---|---|---|---|---|
| Max 0.12 | Max 0.75 | 1.00-1.50 | Max 0.040 | Max 0.015 | 17.0-18.0 | 8.00-9.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 571 (≥) | 445 (≥) | 43 | 22 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 44 | - | - | 0.23 | - | |||
| 316 | 126 | - | 44.3 | 211 | - | ||
| 487 | - | 13 | 32.2 | 421 | 121 | 
Heat treated : 1821°C - 1129°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| Z12CN18-09 | AFNOR | France | Stainless Steel Plate & Steel Strip | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com