France AFNOR Z12CMN17-07Az Stainless Steel Plate & Steel Strip and Z12CMN17-07Az Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z12CMN17-07Az | AFNOR | France | Stainless Steel Plate & Steel Strip | 
| Z6CND18-12-03 | |||||
| Z8CN17 | |||||
| Z8CN25-20 | |||||
| Z8CNT12 | |||||
| Z9CNA17-07 | |||||
| Z10CNDA15-07 | |||||
| Z10NC32-21 | |||||
| Z11CN17-08 | |||||
| Z11CN18-08 | |||||
| Z11CNS17-07Az | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) | 
|---|---|---|---|---|---|---|---|
| Max 0.12 | Max 0.75 | 6.00-7.00 | Max 0.040 | Max 0.015 | 16.0-17.0 | 4.00-5.00 | 0.15-0.20 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 494 (≥) | 827 (≥) | 23 | 21 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.44 | - | |||
| 626 | 183 | - | 43.3 | 132 | - | ||
| 768 | - | 32 | 33.2 | 442 | 323 | 
Heat treated : 1913°C - 1863°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| Z12CMN17-07Az | AFNOR | France | Stainless Steel Plate & Steel Strip | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com