Euronorm EN EN X6NiCrNbCe32-27 Euronorm Stainless Steel and EN X6NiCrNbCe32-27 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X6NiCrNbCe32-27 | EN | Euronorm | Euronorm Stainless Steel | 
| EN XeCrNiMoTi17-12-2 | |||||
| EN X6CrNiNb18-10 | |||||
| EN X6CrNiTi18-10 | |||||
| EN NiCr15Fe8 | |||||
| EN NiCr20Ti | |||||
| EN NiCr22Mo9Nb | |||||
| EN NiCr23Fe | |||||
| EN NiCr28FeSiCe | |||||
| EN X3CrAlTi18-2 | |||||
| EN XSCrNiSiNCe1Mo | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Nb(%) | 
|---|---|---|---|---|---|---|---|
| 0.04-0.08 | Max 0.30 | 1.00 | 0.020 | 0.010 | 26.0-28.0 | 31.0-33.0 | 0.60-1.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 175 (≥) | 997 (≥) | 42 | 24 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.13 | - | |||
| 869 | 697 | - | 21.3 | 222 | - | ||
| 898 | - | 12 | 34.2 | 143 | 144 | 
Heat treated : 1238°C - 1115°C
| Grade | Standard | Country | Application | 
|---|---|---|---|