Euronorm EN EN X3CrAlTi18-2 Euronorm Stainless Steel and EN X3CrAlTi18-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X3CrAlTi18-2 | EN | Euronorm | Euronorm Stainless Steel | 
| EN X6Cr17 | |||||
| EN X6CrAl13 | |||||
| EN XeCrNiMoTi17-12-2 | |||||
| EN X6CrNiNb18-10 | |||||
| EN X6CrNiTi18-10 | |||||
| EN NiCr15Fe8 | |||||
| EN NiCr20Ti | |||||
| EN NiCr22Mo9Nb | |||||
| EN NiCr23Fe | |||||
| EN NiCr28FeSiCe | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ti(%) | 
|---|---|---|---|---|---|---|
| Max 0.04 | Max 1.00 | 1.00 | 0.040 | 0.015 | 17.0-18.0 | 0.20+4(CfN) Max 0.8 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 489 (≥) | 584 (≥) | 12 | 42 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.14 | - | |||
| 418 | 173 | - | 44.3 | 313 | - | ||
| 381 | - | 23 | 42.2 | 324 | 221 | 
Heat treated : 1752°C - 1817°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X3CrAlTi18-2 | EN | Euronorm | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com