Euronorm EN EN NiCr23Fe Euronorm Stainless Steel and EN NiCr23Fe Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN NiCr23Fe | EN | Euronorm | Euronorm Stainless Steel | 
| EN XSCrNiCuNb16-4 | |||||
| EN X5CrNiMo17-12-2 | |||||
| EN X6Cr17 | |||||
| EN X6CrAl13 | |||||
| EN XeCrNiMoTi17-12-2 | |||||
| EN X6CrNiNb18-10 | |||||
| EN X6CrNiTi18-10 | |||||
| EN NiCr15Fe8 | |||||
| EN NiCr20Ti | |||||
| EN NiCr22Mo9Nb | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|
| 0.03-0.10 | Max 0.50 | 100 | 0.020 | 0.015 | 21.0-25.0 | 58.0-63.0 | Max 0.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 231 (≥) | 995 (≥) | 11 | 14 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 444 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.13 | - | |||
| 263 | 386 | - | 14.3 | 221 | - | ||
| 112 | - | 22 | 24.2 | 441 | 331 | 
Heat treated : 1373°C - 1757°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN NiCr23Fe | EN | Euronorm | Euronorm Stainless Steel | 