Euronorm EN EN C5NiCrAlTi31-20 Euronorm Stainless Steel and EN C5NiCrAlTi31-20 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN C5NiCrAlTi31-20 | EN | Euronorm | Euronorm Stainless Steel | 
| EN X2CrTi17 | |||||
| EN X2CrTiNb18 | |||||
| EN X3CrNiMo13-4 | |||||
| EN X3CrNiMo17-13-3 | |||||
| EN X3CrNiMoBN17-13-3 | |||||
| EN X3CrTi17 | |||||
| EN X4CrNtMo16-5-1 | |||||
| EN X5CrNil8-10 | |||||
| EN XSCrNiMo17-12-2 | |||||
| EN X5CrNiN19-9 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Nb(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|---|
| 0.03-0.08 | 0.70 | 1.50 | 0.015 | 0.010 | 19.0-22.0 | 30.0-32.5 | Max 0.10 | 0.20-0.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 226 (≥) | 129 (≥) | 34 | 24 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 32 | - | - | 0.31 | - | |||
| 748 | 724 | - | 33.3 | 113 | - | ||
| 628 | - | 24 | 14.2 | 321 | 441 | 
Heat treated : 1543°C - 1195°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN C5NiCrAlTi31-20 | EN | Euronorm | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com