B 160 N02200

Description

USA ASTM B 160 (2005), B 160 N02200 Superalloys Standard Specification for Nickel Rod and Bar and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: B 160 N02200
Category Class Grade Standard Country Application
Steel GradesSuperalloys B 160 N02200 ASTM USA Standard Specification for Nickel Rod and Bar

Chemical composition(mass fraction)(wt.%) of the B 160 N02200

C Cu Fe Mn C Si S
99.0 - ≥ ≤0.25 ≤0.40 ≤0.35 ≤0.02 ≤0.35 ≤0.01

Mechanical Properties of steel grade B 160 N02200

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
354 (≥) 484 (≥) 13 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical Properties of steel grade B 160 N02200

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
12 - -     0.11 -  
533 168 - 43.3 214   -  
882 - 22 33.2   432 333

Heat Treatment of steel grade B 160 N02200

Heat treated : 1447°C - 1443°C

Technological Curves of steel grade B 160 N02200

Relevant standard of B 160 N02200

B 160 (2005) Standard Specification for Nickel Rod and Bar B-160-(2005).pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this B 160 N02200?
  • List your company on S&G now? Join
  • Non-paying users only
Top