USA ASTM SAE AMS 5342E (2006) , SAE AMS 5343E (2006) , SAE AMS 5344F (2007) , SAE AMS 5604G (2013) , SAE AMS 5622F (2013) , SAE AMS 5643/H1150 (2013) , SAE AMS 5643S (2013) , 17-4PH Specialsteel Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | 17-4PH | Precipitation-Hardening | ASTM | USA | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) | 
| C | Si | Mn | Cr | Ni | Cu | Nb | 
|---|---|---|---|---|---|---|
| ≤0.07 | ≤1.00 | ≤1.00 | 15.00 -17.50 | 3.00 -5.00 | 3.00 -5.00 | 0.15 -1.45 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 346 (≥) | 435 (≥) | 14 | 31 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.44 | - | |||
| 898 | 486 | - | 32.3 | 412 | - | ||
| 924 | - | 21 | 23.2 | 324 | 241 | 
Heat treated : 1134°C - 1257°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| 17-4PH | |||
| 17-4PH | |||
| 17-4PH(630) Steel for Turbine Blades | 
| SAE AMS 5342E (2006) | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) | SAE-AMS-5342E-(2006)-.pdf | 
| SAE AMS 5343E (2006) | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1000) 150 ksi (1034 MPa) Tensile Strength (17-4) | SAE-AMS-5343E-(2006)-.pdf | 
| SAE AMS 5344F (2007) | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H900) 180 ksi (1241 MPa) Tensile Strength (17-4) | SAE-AMS-5344F-(2007)-.pdf | 
| SAE AMS 5604G (2013) | Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr - 4.0Ni - 4.0Cu - 0.30Cb Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5604G-(2013)-.pdf | 
| SAE AMS 5622F (2013) | Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted | SAE-AMS-5622F-(2013)-.pdf | 
| SAE AMS 5643/H1150 (2013) | Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing and Rings 16Cr – 4.0Ni – 0.30Cb (Nb) – 4.0Cu Solution and Precipitation Heat Treated (H1150) | SAE-AMS-5643-H1150-(2013)-.pdf | 
| SAE AMS 5643S (2013) | Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5643S-(2013)-.pdf | 