| SKT3 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | 
|---|---|---|---|---|---|---|---|
| 0.50-0.60 | 0.10-0.40 | 0.60-0.90 | Max 0.030 | Max 0.020 | 0.80-1.20 | 0.35-0.55 | 0.05-0.15 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 717 (≥) | 479 (≥) | 32 | 34 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.23 | - | |||
| 267 | 698 | - | 22.3 | 344 | - | ||
| 578 | - | 41 | 31.2 | 322 | 431 | 