Japan JIS SKD7 Hot-work die steel and SKD7 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | SKD7 | JIS | Japan | Hot-work die steel | 
| SKD1 | |||||
| SKD2 | |||||
| SKD10 | |||||
| SKD11 | |||||
| SKD12 | |||||
| SKD4 | |||||
| SKD5 | |||||
| SKD6 | |||||
| SKD61 | |||||
| SKD62 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | 
|---|---|---|---|---|---|---|---|
| 0.28-0.35 | 0.10-0.40 | 0.15-0.45 | Max 0.030 | Max 0.020 | 2.70-3.20 | 2.50-3.00 | 0.40-0.70 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 377 (≥) | 467 (≥) | 13 | 21 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.34 | - | |||
| 593 | 756 | - | 33.3 | 423 | - | ||
| 826 | - | 31 | 44.2 | 114 | 231 | 
Heat treated : 1644°C - 1787°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...