USA ASTM H24 Alloy tool steel and H24 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | H24 | ASTM | USA | Alloy tool steel | 
| H14 | |||||
| T20814 | |||||
| H19 | |||||
| T20819 | |||||
| H21 | |||||
| T20821 | |||||
| H22 | |||||
| T20822 | |||||
| H23 | |||||
| T20823 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | V(%) | W(%) | 
|---|---|---|---|---|---|---|---|
| 0.42~0.53 | 0.15~0.40 | 0.15~0.40 | ≤0.030 | ≤0.030 | 2.50~3.50 | 0.40~0.60 | 14.0~16.0 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 891 (≥) | 387 (≥) | 12 | 24 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 413 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 42 | - | - | 0.21 | - | |||
| 965 | 212 | - | 21.3 | 421 | - | ||
| 418 | - | 34 | 23.2 | 432 | 342 | 
Heat treated : 1129°C - 1184°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| H24 | ASTM | USA | Alloy tool steel | 
| 08X15H24Φ4TP | Austenitic | ||
| 08X15H24Φ4TP | ГОСТ | Russia | Austenitic steel | 
| SWRCH24K | CNS | China | China Taiwan Structural steel | 
| EN H240LA | EN | Euronorm | Euronorm Structural steel | 