Germany DIN 1.2889 Hot working alloy tool steel and 1.2889 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | 1.2889 | DIN | Germany | Hot working alloy tool steel | 
| 1.2786 | |||||
| X23CrNi17 | |||||
| 1.2787 | |||||
| X32CrMoCoV3-3-3 | |||||
| 1.2885 | |||||
| X15CrMoCoV10-10-5 | |||||
| 1.2886 | |||||
| X20CoCrWMo10-9 | |||||
| 1.2888 | |||||
| X45CoCrMoV5-5-3 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | Co(%) | 
|---|---|---|---|---|---|---|---|---|
| 0.40-0.50 | 0.30-0.50 | 0.30-0.50 | Max 0.025 | Max 0.025 | 4.00-5.00 | 2.80-3.30 | 1.80-2.10 | 4.00-5.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 141 (≥) | 152 (≥) | 11 | 13 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 33 | - | - | 0.13 | - | |||
| 748 | 368 | - | 12.3 | 432 | - | ||
| 184 | - | 31 | 12.2 | 313 | 113 | 
Heat treated : 1498°C - 1645°C