France AFNOR Z4C17FF Cold drawn stainless steel bar and wire rod(NF A 35-577(1990)) and Z4C17FF Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z4C17FF | AFNOR | France | Cold drawn stainless steel bar and wire rod(NF A 35-577(1990)) | 
| Z10C3 | |||||
| Z11CF13 | |||||
| Z12CND16-05-03 | |||||
| Z13CF17 | |||||
| Z15CN16-02 | |||||
| Z29CF13 | |||||
| Z3CN19-11FF | |||||
| Z3CND17-11-02FF | |||||
| Z3CNU18-09FF | |||||
| Z3CNU18-10FF | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | 
|---|---|---|---|---|---|---|---|
| Max 0.04 | Max 1.00 | Max 1.00 | Max 0.040 | Max 0.015 | 16.0-18.0 | Max 0.50 | Max 0.30 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 341 (≥) | 254 (≥) | 42 | 42 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 33 | - | - | 0.31 | - | |||
| 886 | 484 | - | 14.3 | 341 | - | ||
| 168 | - | 44 | 22.2 | 213 | 213 | 
Heat treated : 1615°C - 1311°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| Z4C17FF | AFNOR | France | Cold drawn stainless steel bar and wire rod(NF A 35-577(1990)) | 