France AFNOR X1NiCrMoCuN25-20-7(AFNOR) Austenite and X1NiCrMoCuN25-20-7(AFNOR) Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | X1NiCrMoCuN25-20-7(AFNOR) | AFNOR | France | Austenite | 
| X2CrNiN17-7-5 | |||||
| 1.4371 | |||||
| X12CrMnNiN18-9-5 | |||||
| 1.4373 | |||||
| X1NiMoCu31-27-4 | |||||
| 1.4563(AFNOR) | |||||
| X1CrNiMoCuN25-25-2 | |||||
| 1.4537(AFNOR) | |||||
| X1CrNiMoCuN20-18-7 | |||||
| 1.4547(AFNOR) | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) | 
|---|---|---|---|---|---|---|---|---|---|
| Max 0.020 | Max 0.50 | Max 1.00 | Max 0.030 | Max 0.010 | 19.00-21.00 | 24.00-26.00 | 6.00-7.00 | 0.15-0.25 | 0.50-1.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 425 (≥) | 244 (≥) | 32 | 11 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.34 | - | |||
| 262 | 544 | - | 13.3 | 332 | - | ||
| 628 | - | 13 | 14.2 | 144 | 244 | 
Heat treated : 1884°C - 1548°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| X1NiCrMoCuN25-20-7(AFNOR) | AFNOR | France | Austenite | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com