Romania STAS/SR T12NNiCrl90 Cast Steel and T12NNiCrl90 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | T12NNiCrl90 | STAS/SR | Romania | Cast Steel | 
| S28MnlCr12MolVW11. 5 | 
                                |||||
| S32MoCr6 | 
                                |||||
| S40CrMnlSil | 
                                |||||
| S55MoCr6 | 
                                |||||
| S80Cr | 
                                |||||
| T7MoNiCrl80 | 
                                |||||
| T7NiCrl80 | 
                                |||||
| T8MoNiCrlZ5 | 
                                |||||
| T12MoNiCr210 | 
                                |||||
| T12NiCr210 | 
                                
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) | 
|---|---|---|---|---|---|---|---|
| 0.12 | ≤1.50 | 2.00 | 0.035 | 0.030 | 18.0-20.0 | 6.00-8.00 | 0.10-0.20 | 
| Yield Rp0.2 (MPa)  | 
                                            Tensile Rm (MPa)  | 
                                            Impact KV/Ku (J)  | 
                                            Elongation A (%)  | 
                                            Reduction in cross section on fracture Z (%)  | 
                                            As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 792 (≥) | 511 (≥) | 21 | 14 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | 
| Temperature (°C)  | 
                                        Modulus of elasticity (GPa)  | 
                                        Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C)  | 
                                        Specific thermal capacity (J/kg·°C)  | 
                                        Specific electrical resistivity (Ω mm²/m)  | 
                                        Density (kg/dm³)  | 
                                        Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.44 | - | |||
| 273 | 984 | - | 34.3 | 232 | - | ||
| 451 | - | 43 | 34.2 | 212 | 241 | 
Heat treated : 1972°C - 1725°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| T12NNiCrl90 | STAS/SR | Romania | Cast Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...