Japan JIS SUS304L austenitic special steel and SUS304L Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | SUS304L | JIS | Japan | austenitic special steel | 
| SUS316TKA | |||||
| SUS321TKA | |||||
| SUS347TKA | |||||
| SUS410TKA | |||||
| SUS410TKC | |||||
| SUS420J1TKA | |||||
| SUS420J2TKA | |||||
| SUS430TKA | |||||
| SUS430TKC | |||||
| SUS304 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | 
|---|---|---|---|---|---|---|
| Max 0.030 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.03 | 18.0- 20.0 | 9.00- 13.0 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 412 (≥) | 171 (≥) | 32 | 34 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.33 | - | |||
| 818 | 489 | - | 33.3 | 421 | - | ||
| 275 | - | 13 | 42.2 | 112 | 433 | 
Heat treated : 1466°C - 1729°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| SUS304LFB | JIS | Japan | austenitic special steel | 
| SUS304LTP | JIS | Japan | austenitic special steel | 
| SUS304L | JIS | Japan | austenitic special steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...