Japan JIS SUS430TKC ferritic stainless steel and SUS430TKC Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | SUS430TKC | JIS | Japan | ferritic stainless steel | 
| SUS304TKA | |||||
| SUS304TKC | |||||
| SUS316TKA | |||||
| SUS321TKA | |||||
| SUS347TKA | |||||
| SUS410TKA | |||||
| SUS410TKC | |||||
| SUS420J1TKA | |||||
| SUS420J2TKA | |||||
| SUS430TKA | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | 
|---|---|---|---|---|---|---|
| Max 0.12 | Max 0.75 | Max 1.00 | Max 0.04 | Max 0.03 | 16.00-18.00 | Max 0.60 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 539 (≥) | 335 (≥) | 44 | 34 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.34 | - | |||
| 378 | 786 | - | 33.3 | 223 | - | ||
| 645 | - | 11 | 42.2 | 442 | 133 | 
Heat treated : 1233°C - 1367°C