Euronorm EN EN X8Cr17KD Euronorm Stainless Steel and EN X8Cr17KD Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X8Cr17KD | EN | Euronorm | Euronorm Stainless Steel | 
| EN X8NiCrAlTi32-20 | |||||
| EN X10CrNiMoMnNbVB15-10-1 | |||||
| EN X2CrNiNi810KD | |||||
| EN X2CrNiMoNi8133KD | |||||
| EN X3CrNi1810KD | |||||
| EN X3CrNiMo17122KD | |||||
| EN X6CrNi1S10KD | |||||
| EN X6CrNiMo17122KD | |||||
| EN X6CrNiCu18104KD | |||||
| EN X6NiCr181GKD | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 198 (≥) | 578 (≥) | 21 | 12 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.34 | - | |||
| 819 | 382 | - | 12.3 | 234 | - | ||
| 131 | - | 34 | 23.2 | 431 | 133 | 
Heat treated : 1836°C - 1919°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X8Cr17KD | EN | Euronorm | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com