Euronorm EN EN X3CrNiMo17122KD Euronorm Stainless Steel and EN X3CrNiMo17122KD Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X3CrNiMo17122KD | EN | Euronorm | Euronorm Stainless Steel | 
| EN X6CrNiNb18-10 | |||||
| EN X6CrNiTi18-10 | |||||
| EN X7CrNiTiB18-10 | |||||
| EN X8CrNiM0VNb16-13 | |||||
| EN X8CrNiNb16-13 | |||||
| EN X8NiCrAlTi32-20 | |||||
| EN X10CrNiMoMnNbVB15-10-1 | |||||
| EN X2CrNiNi810KD | |||||
| EN X2CrNiMoNi8133KD | |||||
| EN X3CrNi1810KD | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | 
|---|---|---|---|---|---|---|---|
| 0.03 | 1.00 | 2.00 | 0.045 | 0.030 | 16.0-18.5 | 10.5-13.5 | 2.00-2.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 562 (≥) | 537 (≥) | 12 | 31 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.33 | - | |||
| 652 | 125 | - | 32.3 | 142 | - | ||
| 853 | - | 44 | 14.2 | 133 | 341 | 
Heat treated : 1861°C - 1663°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X3CrNiMo17122KD | EN | Euronorm | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...