Euronorm EN EN X6CrNiNb2010KE Euronorm Stainless Steel and EN X6CrNiNb2010KE Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X6CrNiNb2010KE | EN | Euronorm | Euronorm Stainless Steel | 
| EN X6NiCr181GKD | |||||
| EN X8Cr17KD | |||||
| EN X8CrNi1812KD | |||||
| EN X12Cr13KD | |||||
| EN X2CrNi2010KE | |||||
| EN X2CrNi2413KE | |||||
| EN X2CrNiMo191303KE | |||||
| EN X2CrNiMnMoN201508KE | |||||
| EN X3CrNi1404KE | |||||
| EN X4Cr13KE | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Nb(%) | 
|---|---|---|---|---|---|---|---|---|---|
| 0.06 | 0.55 | 1.10-1.90 | 0.025 | 0.015 | 18.2-20.8 | 9.20-10.8 | Max 0.47 | 0.47 | 10XCMax 0.95 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 939 (≥) | 621 (≥) | 13 | 31 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 113 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 33 | - | - | 0.13 | - | |||
| 352 | 156 | - | 21.3 | 234 | - | ||
| 678 | - | 21 | 12.2 | 213 | 212 | 
Heat treated : 1819°C - 1378°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X6CrNiNb2010KE | EN | Euronorm | Euronorm Stainless Steel | 