Germany DIN 2.4631 The high-temperature and high-strength steel and 2.4631 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | 2.4631 | DIN | Germany | The high-temperature and high-strength steel | 
| X6CrNiWNb16-16 | |||||
| 1.4945 | |||||
| 1.4948 | |||||
| X6CrNiTiB18-10/X8CrNiTi18-10 | |||||
| X3CrNiN18-11 | |||||
| 1.4949 | |||||
| NiCr20Ti | |||||
| 2.4951 | |||||
| NiCr20TiAl | |||||
| 2.4952 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | 
|---|---|---|---|---|---|---|
| 0.04-0.10 | Max 1.00 | Max 1.00 | Max 0.020 | Max 0.015 | 18.0-21.0 | Mix 65.0 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 827 (≥) | 779 (≥) | 13 | 42 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 121 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.42 | - | |||
| 415 | 525 | - | 31.3 | 132 | - | ||
| 423 | - | 24 | 11.2 | 234 | 231 | 
Heat treated : 1765°C - 1115°C