Global 企业标准 VIDAR1 Bohler-Uddeholm AG and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: VIDAR1 / VIDAR 1
Category Grade Standard Region/Area Standard Content
Metals VIDAR 1 -- Global Bohler-Uddeholm AG

Chemical composition(mass fraction)(wt.%) of the VIDAR 1

Element Min Max Similar
V - 0.4000 -
Si - 1.0000 -
Mo - 1.3000 -
Mn - 0.4000 -
Cr - 5.0000 -
C - 0.3800 -

Mechanical Properties of steel grade VIDAR 1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
692 (≥) 412 (≥) 23 14 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical Properties of steel grade VIDAR 1

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
11 - -     0.21 -  
293 926 - 22.3 342   -  
549 - 34 32.2   211 441

Heat Treatment of steel grade VIDAR 1

Heat treated : 1956°C - 1843°C

Technological Curves of steel grade VIDAR 1

Cross Reference Table (Equivalent Grade) of VIDAR 1

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this VIDAR 1?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top