Available 24/7 at contact@steel-grades.com

Germany DIN 2.3710 Tin alloy for table plate (pewter); chemical composition and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: 2.3710 / 2.3710
Category Grade Standard Region/Area Standard Content
Metals 2.3710 DIN 17810 Germany Tin alloy for table plate (pewter); chemical composition

Chemical composition(mass fraction)(wt.%) of the 2.3710

Element Min Max Similar

Mechanical Properties of steel grade 2.3710

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
653 (≥) 374 (≥) 13 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical Properties of steel grade 2.3710

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.31 -  
388 822 - 23.3 444   -  
712 - 43 14.2   334 334

Heat Treatment of steel grade 2.3710

Heat treated : 1887°C - 1576°C

Technological Curves of steel grade 2.3710

Cross Reference Table (Equivalent Grade) of 2.3710

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 2.3710?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top