Germany DIN 2.1322 Low alloy wrought copper alloys - Composition and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: 2.1322 / 2.1322
Category Grade Standard Region/Area Standard Content
Metals 2.1322 DIN 17666 Germany Low alloy wrought copper alloys - Composition

Chemical composition(mass fraction)(wt.%) of the 2.1322

Element Min Max Similar
Tot. other - 0.3000 -
Mg 0.5000 0.8000 -
Cu - - -

Mechanical Properties of steel grade 2.1322

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
893 (≥) 459 (≥) 44 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical Properties of steel grade 2.1322

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
14 - -     0.44 -  
927 366 - 33.3 414   -  
455 - 42 11.2   214 434

Heat Treatment of steel grade 2.1322

Heat treated : 1331°C - 1262°C

Technological Curves of steel grade 2.1322

Cross Reference Table (Equivalent Grade) of 2.1322

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 2.1322?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top