India IS GWCuSn7 Phosphor bronze ingots and castings and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: GWCuSn7 / GW CuSn7
Category Grade Standard Region/Area Standard Content
Metals GW CuSn7 IS 28 India Phosphor bronze ingots and castings

Chemical composition(mass fraction)(wt.%) of the GW CuSn7

Element Min Max Similar

Mechanical Properties of steel grade GW CuSn7

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
245 (≥) 884 (≥) 12 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical Properties of steel grade GW CuSn7

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
14 - -     0.33 -  
651 364 - 33.3 314   -  
856 - 11 24.2   421 443

Heat Treatment of steel grade GW CuSn7

Heat treated : 1357°C - 1737°C

Technological Curves of steel grade GW CuSn7

Cross Reference Table (Equivalent Grade) of GW CuSn7

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this GW CuSn7?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top