Korea KS TAW6400 Titanium and titanium alloys-Wires and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: TAW6400 / TAW 6400
Category Grade Standard Region/Area Standard Content
Metals TAW 6400 KS D 5576 Korea Titanium and titanium alloys-Wires

Chemical composition(mass fraction)(wt.%) of the TAW 6400

Element Min Max Similar

Mechanical Properties of steel grade TAW 6400

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
143 (≥) 443 (≥) 11 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical Properties of steel grade TAW 6400

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
34 - -     0.43 -  
554 727 - 42.3 341   -  
781 - 32 44.2   442 121

Heat Treatment of steel grade TAW 6400

Heat treated : 1348°C - 1357°C

Technological Curves of steel grade TAW 6400

Cross Reference Table (Equivalent Grade) of TAW 6400

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this TAW 6400?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top