Available 24/7 at contact@steel-grades.com

KOSIL 200 S

Global 企业标准 KOSIL200S and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: KOSIL200S / KOSIL 200 S
Category Grade Standard Region/Area Standard Content
Metals KOSIL 200 S -- Global

Chemical composition(mass fraction)(wt.%) of the KOSIL 200 S

Element Min Max Similar
Si - 0.0300 -
S - 0.0200 -
P - 0.0250 -
Mn - 0.6000 -
C - 0.1600 -

Mechanical Properties of steel grade KOSIL 200 S

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
695 (≥) 516 (≥) 24 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical Properties of steel grade KOSIL 200 S

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
23 - -     0.13 -  
712 414 - 14.3 244   -  
934 - 41 42.2   242 132

Heat Treatment of steel grade KOSIL 200 S

Heat treated : 1363°C - 1325°C

Technological Curves of steel grade KOSIL 200 S

Cross Reference Table (Equivalent Grade) of KOSIL 200 S

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this KOSIL 200 S?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top