Available 24/7 at contact@steel-grades.com

Outokumpu SAF 2507

Global 企业标准 OutokumpuSAF2507 and Mechanical Properties, Chemical Element, Cross Reference.

Category Grade Standard Region/Area Standard Content
Metals Outokumpu SAF 2507 -- Global

Chemical composition(mass fraction)(wt.%) of the Outokumpu SAF 2507

Element Min Max Similar

Mechanical Properties of steel grade Outokumpu SAF 2507

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
511 (≥) 639 (≥) 14 33 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical Properties of steel grade Outokumpu SAF 2507

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
42 - -     0.32 -  
114 684 - 33.3 143   -  
832 - 21 11.2   344 422

Heat Treatment of steel grade Outokumpu SAF 2507

Heat treated : 1981°C - 1453°C

Technological Curves of steel grade Outokumpu SAF 2507

Cross Reference Table (Equivalent Grade) of Outokumpu SAF 2507

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this Outokumpu SAF 2507?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top