Available 24/7 at contact@steel-grades.com

SB-637 N07750 Type 1

Description

USA ASME SB-637, SB-637 N07750 Type 1 Superalloys Precipitation-Hardening Nickel Alloy Bars, Forgings, and Forging Stock for High-Temperature Service and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: SB-637 N07750 Type 1
Category Class Grade Standard Country Application
Steel GradesSuperalloys SB-637 N07750 Type 1 ASME USA Precipitation-Hardening Nickel Alloy Bars, Forgings, and Forging Stock for High-Temperature Service

Chemical composition(mass fraction)(wt.%) of the SB-637 N07750 Type 1

C Mn Si S P Cu Fe Co Nb Cr Ni Al Ti
≤0.08 ≤1.0 ≤0.5 ≤0.01 ≤0.015 ≤0.5 5.0 -9.0 ≤1.0 0.70 -1.20 14.0 -17.0 70 - ≥ 0.40 -1.00 2.25 -2.75

Mechanical Properties of steel grade SB-637 N07750 Type 1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
949 (≥) 164 (≥) 42 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical Properties of steel grade SB-637 N07750 Type 1

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
12 - -     0.13 -  
844 878 - 21.3 222   -  
319 - 32 13.2   334 412

Heat Treatment of steel grade SB-637 N07750 Type 1

Heat treated : 1313°C - 1541°C

Technological Curves of steel grade SB-637 N07750 Type 1

Cross Reference Table (Equivalent Grade) of SB-637 N07750 Type 1

Relevant standard of SB-637 N07750 Type 1

SB-637 Precipitation-Hardening Nickel Alloy Bars, Forgings, and Forging Stock for High-Temperature Service SB-637.pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this SB-637 N07750 Type 1?
  • List your company on S&G now? Join
  • Non-paying users only
Top