B 637 N07750 Type 1

Description

USA ASTM B 637 (2012), B 637 N07750 Type 1 Superalloys Precipitation-Hardening and Cold Worked Nickel Alloy Bars, Forgings, and Forging Stock for Moderate or High Temperature Service and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: B 637 N07750 Type 1
Category Class Grade Standard Country Application
Steel GradesSuperalloys B 637 N07750 Type 1 ASTM USA Precipitation-Hardening and Cold Worked Nickel Alloy Bars, Forgings, and Forging Stock for Moderate or High Temperature Service

Chemical composition(mass fraction)(wt.%) of the B 637 N07750 Type 1

C Mn Si S P Cu Fe Co Nb Cr Ni Al Ti
≤0.08 ≤1.0 ≤0.5 ≤0.01 ≤0.015 ≤0.5 5.0 -9.0 ≤1.0 0.70 -1.20 14.0 -17.0 70 - ≥ 0.40 -1.00 2.25 -2.75

Mechanical Properties of steel grade B 637 N07750 Type 1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
616 (≥) 264 (≥) 22 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical Properties of steel grade B 637 N07750 Type 1

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
24 - -     0.33 -  
576 892 - 24.3 433   -  
831 - 12 42.2   313 314

Heat Treatment of steel grade B 637 N07750 Type 1

Heat treated : 1149°C - 1553°C

Technological Curves of steel grade B 637 N07750 Type 1

Cross Reference Table (Equivalent Grade) of B 637 N07750 Type 1

Relevant standard of B 637 N07750 Type 1

B 637 (2012) Precipitation-Hardening and Cold Worked Nickel Alloy Bars, Forgings, and Forging Stock for Moderate or High Temperature Service B-637-(2012).pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this B 637 N07750 Type 1?
  • List your company on S&G now? Join
  • Non-paying users only
Top