NiCr23Mo16Al

Description

European EN DIN EN 17744, NiCr23Mo16Al Superalloys The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry. and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: NiCr23Mo16Al
Category Class Grade Standard Country Application
Steel GradesSuperalloys NiCr23Mo16Al EN European The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.

Chemical composition(mass fraction)(wt.%) of the NiCr23Mo16Al

C Si Mn P S Cr Ni Al Co Cu Fe
≤0.01 ≤0.10 ≤0.50 ≤0.025 ≤0.015 22.00 -24.00 ≤Bal 0.10 -0.40 ≤0.30 ≤0.50 ≤1.50

Mechanical Properties of steel grade NiCr23Mo16Al

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
533 (≥) 511 (≥) 24 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical Properties of steel grade NiCr23Mo16Al

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
33 - -     0.43 -  
155 491 - 21.3 224   -  
634 - 11 24.2   143 333

Heat Treatment of steel grade NiCr23Mo16Al

Heat treated : 1837°C - 1331°C

Technological Curves of steel grade NiCr23Mo16Al

Relevant standard of NiCr23Mo16Al

DIN EN 17744 The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry. DIN-EN-17744.pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this NiCr23Mo16Al?
  • List your company on S&G now? Join
  • Non-paying users only
Top