Available 24/7 at contact@steel-grades.com
  • Incoloy 800
  • Steel type: Superalloys
  • Country/Region: USA - UNS
  • Standard: ASTM B409 - Stainless steel hot rolled steel plate
  • Description: Equipment used in the manufacture of resistance to stress corrosion cracking
  • GH 3536
  • Steel type: Superalloys
  • Country/Region: China - JB
  • Description: Superalloy GH536 is a kind of added tungsten cobalt and nickel - chromium - molybdenum alloy.GH536 alloy at 1200 ℃ with excellent oxidation resistance at high temperature, also can be applied to the neutral and reducing atmosphere.At the same time GH536 a
  • X6NiCrTiMoVB25-15-2
  • Steel type: Superalloys
  • Country/Region: European - EN
  • Standard: EN 10302: 2008 - Creep resisting steels, nickel and cobalt alloys
  • Description: Creep resisting steels, nickel and cobalt alloys
  • 1.4980
  • Steel type: Superalloys
  • Country/Region: European - EN
  • Standard: EN 10302: 2008 - Creep resisting steels, nickel and cobalt alloys
  • Description: Creep resisting steels, nickel and cobalt alloys
  • MONEL ALLOY 400
  • Steel type: Superalloys
  • Country/Region: USA - UNS
  • Standard: UNS N04400 -
  • Description: Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • ALLOY 301
  • Steel type: Superalloys
  • Country/Region: USA - UNS
  • Standard: UNS N03301 - Round bar and wire.
  • Description: An age-hardened alloy that combines the excellent corrosion resistance characteristics of Nickel 200 with the added advantages of greater strength and hardness.
  • NICKEL 201
  • Steel type: Superalloys
  • Country/Region: USA - ASTM
  • Standard: UNS N02201 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • Description: Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • NiCr23Mo16Al
  • Steel type: Superalloys
  • Country/Region: European - EN
  • Standard: DIN EN 17744 - The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.
  • Description: The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.
  • Alloy 59
  • Steel type: Superalloys
  • Country/Region: USA - ASTM
  • Standard: DIN EN 17744 - The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.
  • Description: The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.
  • 2.4605
  • Steel type: Superalloys
  • Country/Region: Germany - DIN
  • Standard: DIN EN 17744 - The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.
  • Description: The chemically stable and high-temperature resistant nickel and cobalt alloy 2.4605 (alloy 59) is mainly used in the chemical industry, flue gas desulphurating plants, paper industry.
  • GH3652
  • Steel type: Superalloys
  • Country/Region: China - GB
  • Standard: GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials
  • Description: Classification and designation for superalloys and high temperature intermetallic materials
  • 18Ni Maraging Steel
  • Steel type: Superalloys
  • Country/Region: USA - ASTM
  • Standard: AMS 6514 -
  • Description: Typical applications for maraging include missile and rocket motor cases, landing and takeoff gear, munitions, aerospace, extrusion tooling, die casting, high performance shafting, gears and fasteners.
  • Inconel 722
  • Steel type: Superalloys
  • Country/Region: USA - AMS
  • Standard: AMS 5411 - Nickel Inconel 722 AMS 5541 Strip
  • Description: Used for gas turbine structural components, such as turbine section frames. The alloy is useful where oxidation resistance and high temperature strength are of major importance.
Top