Korea KS D 3702 (2008), D 3706 (2008), STS431 Specialsteel Stainless steel bars and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | STS431 | Martensite | KS | Korea | Stainless steel bars | 
| C | Si | Mn | P | S | Cr | Ni | Mo | N | 
|---|---|---|---|---|---|---|---|---|
| ≤0.20 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.030 | 15.00 -17.00 | 1.25 -2.50 | ≤ ≥ | ≤ ≥ | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 432 (≥) | 338 (≥) | 13 | 24 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.44 | - | |||
| 744 | 793 | - | 44.3 | 123 | - | ||
| 324 | - | 33 | 41.2 | 112 | 423 | 
Heat treated : 1474°C - 1213°C
| D 3702 (2008) | Stainless steel wire rods | D-3702-(2008).pdf | 
| D 3706 (2008) | Stainless steel bars | D-3706-(2008).pdf | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com