Korea KS D 3576 (2011), D 9536 (2011), STS316TiTP Specialsteel Stainless lined steel pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application |
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | STS316TiTP | Austenite | KS | Korea | Stainless lined steel pipe |
| C | Si | Mn | P | S | Cr | Ni | Mo | N | Ti |
|---|---|---|---|---|---|---|---|---|---|
| ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 16.00 -18.00 | 10.00 -14.00 | 2.00 -3.00 | ≤ ≥ | 5×C% - ≥ |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 123 (≥) | 585 (≥) | 44 | 34 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.32 | - | |||
| 339 | 287 | - | 44.3 | 413 | - | ||
| 794 | - | 21 | 32.2 | 122 | 422 |
Heat treated : 1795°C - 1653°C
| D 3576 (2011) | Stainless steel pipes | D-3576-(2011).pdf |
| D 9536 (2011) | Stainless lined steel pipe | D-9536-(2011).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com