Russia GOST 08X18ΦБ Specialsteel Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | 08X18ΦБ | Austenite | GOST | Russia | Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition | 
| C | Si | Mn | P | S | Cr | Ni | Mo | W | Ti | 
|---|---|---|---|---|---|---|---|---|---|
| 0.06 -0.12 | ≤0.80 | ≤2.00 | ≤0.025 | ≤0.025 | 17.00 -19.00 | ≤0.60 | ≤0.30 | ≤0.20 | 5×C -0.60 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 364 (≥) | 279 (≥) | 14 | 33 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.42 | - | |||
| 146 | 848 | - | 21.3 | 132 | - | ||
| 328 | - | 23 | 21.2 | 331 | 421 | 
Heat treated : 1978°C - 1966°C