France AFNOR NF A 35-595, Z11CN18-08CI Specialsteel Iron and steel. Cutlery stainless steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Specialsteel | Z11CN18-08CI | AFNOR | France | Iron and steel. Cutlery stainless steel |
| C | Si | Mn | P | S | Cr | Mo | Ni |
|---|---|---|---|---|---|---|---|
| 0.09 -0.12 | ≤0.75 | 0.75 -1.20 | ≤0.040 | ≤0.015 | 16.50 -18.50 | ≤ ≥ | 7.00 -8.00 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 226 (≥) | 728 (≥) | 23 | 42 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.24 | - | |||
| 364 | 394 | - | 21.3 | 433 | - | ||
| 676 | - | 33 | 42.2 | 344 | 144 |
Heat treated : 1318°C - 1599°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| Z11CN18-08 | |||
| Z11CN18-08 |
| NF A 35-595 | Iron and steel. Cutlery stainless steel | NF-A-35-595.pdf |