UK B.S. BS 2901-5, NA37 Specialsteel Filler rods and wires for gas-shielded arc welding; Nickel and nickel alloys and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Specialsteel | NA37 | B.S. | UK | Filler rods and wires for gas-shielded arc welding; Nickel and nickel alloys | 
| C | Si | Mn | P | S | Cr | Mo | Ni | Cu | 
|---|---|---|---|---|---|---|---|---|
| ≤0.15 | 3.50 -4.50 | ≤1.50 | ≤0.030 | ≤0.030 | ≤ ≥ | ≤ ≥ | ≤remaining | 28.00 -34.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 114 (≥) | 396 (≥) | 23 | 42 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.43 | - | |||
| 211 | 868 | - | 12.3 | 133 | - | ||
| 682 | - | 21 | 43.2 | 224 | 112 | 
Heat treated : 1554°C - 1231°C
| BS 2901-5 | Filler rods and wires for gas-shielded arc welding; Nickel and nickel alloys | BS-2901-5.pdf | 