USA UNS SAE AMS 7726G (2000), Kovar Specialsteel Iron-Nickel-Cobalt Alloy, Wire 53Fe - 29Ni - 17Co Low Expansion, Glass Sealing, Annealed and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | Kovar | Precipitation-Hardening | UNS | USA | Iron-Nickel-Cobalt Alloy, Wire 53Fe - 29Ni - 17Co Low Expansion, Glass Sealing, Annealed | 
| C | Si | Mn | Ni | Cr | Al | Cu | Ti | Fe | Mo | Co | W | Mg | Zr | 
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ≤0.04 | ≤0.20 | ≤0.50 | ≤29.00 | ≤0.20 | ≤0.10 | ≤0.20 | ≤0.10 | ≤53.00 | ≤0.20 | ≤17.00 | ≤ ≥ | ≤0.10 | ≤0.10 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 912 (≥) | 215 (≥) | 14 | 12 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.11 | - | |||
| 911 | 462 | - | 13.3 | 441 | - | ||
| 437 | - | 14 | 41.2 | 444 | 213 | 
Heat treated : 1833°C - 1974°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| KOVAR | 
| SAE AMS 7726G (2000) | Iron-Nickel-Cobalt Alloy, Wire 53Fe - 29Ni - 17Co Low Expansion, Glass Sealing, Annealed | SAE-AMS-7726G-(2000).pdf | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com