USA SAE A 928/A 928M (2011), A 928 Type 2507 Specialsteel Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application |
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | A 928 Type 2507 | Precipitation-Hardening | SAE | USA | Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal |
| C | Si | Mn | P | S | Ni | Cr | Al | Cu | Ti | Fe | N | Mo | W | V |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ≤0.03 | ≤0.08 | ≤1.20 | ≤0.035 | ≤0.02 | 6.00 -8.00 | 24.00 -26.00 | ≤ ≥ | ≤ ≥ | ≤ ≥ | ≤ ≥ | 0.24 -0.32 | 3.00 -5.00 | ≤ ≥ | ≤ ≥ |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 689 (≥) | 587 (≥) | 13 | 34 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 41 | - | - | 0.43 | - | |||
| 266 | 797 | - | 31.3 | 221 | - | ||
| 385 | - | 32 | 44.2 | 244 | 434 |
Heat treated : 1893°C - 1859°C
| A 928/A 928M (2011) | Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal | A-928-A-928M-(2011).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com