USA SAE A 493 (2009), A 493 S44625 Specialsteel Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | A 493 S44625 | Ferrite | SAE | USA | Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging | 
| C | Mn | Si | P | S | Cr | Ni | Mo | N | Cu | 
|---|---|---|---|---|---|---|---|---|---|
| ≤0.01 | ≤0.40 | ≤0.40 | ≤0.02 | ≤0.02 | 25.00 -27.00 | ≤0.50 | 0.75 -1.50 | ≤0.015 | 0.20 - ≥ | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 844 (≥) | 295 (≥) | 22 | 11 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 41 | - | - | 0.33 | - | |||
| 534 | 767 | - | 32.3 | 231 | - | ||
| 445 | - | 44 | 33.2 | 433 | 331 | 
Heat treated : 1921°C - 1188°C
| A 493 (2009) | Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging | A-493-(2009).pdf | 