HS10-4-3-10 Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel | HS10-4-3-10 | |||
| 1.2889 | |||||
| X45CrMoCoV5-5-3 | |||||
| NiCr19NbMo | |||||
| NiCr19Fe19Nb5Mo3 | |||||
| 1.4668 | |||||
| 1.4973 | |||||
| NiCr19CoMo | |||||
| 1.3202 | |||||
| S 12-1-4-5 | |||||
| HS12-1-4-5 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| 1.20-1.35 | 0.45 | 0.40 | 0.030 | 0.030 | 3.80-4.50 | 3.20-3.90 | W 9.00-10.0   V 3.00-3.50 Co 9.50-10.5 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 121 (≥) | 328 (≥) | 43 | 12 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.21 | - | |||
| 679 | 885 | - | 22.3 | 214 | - | ||
| 298 | - | 21 | 11.2 | 112 | 141 | 
Heat treated : 1394°C - 1759°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| HS10-4-3-10 | AFNOR | France | Carbide for cutting tools | 
| EN HS10-4-3-10 | EN | Euronorm Tool steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com