1.3257 Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel | 1.3257 | |||
| S2-9-10-8 | |||||
| HS2-9-1-8 | |||||
| S 2-9-2-8 | |||||
| HS2-9-2-8 | |||||
| 1.3249 | |||||
| 1.3255 | |||||
| S 18-1-2-5 | |||||
| HS18-1-2-5 | |||||
| S 18-1-2-15 | |||||
| HS18-1-2-15 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| 0.60-0.70 | 0.45 | 0.40 | 0.030 | 0.030 | 3.80-4.50 | 0.50-1.00 | W 17.5-18.5  V  1.40-1.70 Co 15.0-16.0 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 589 (≥) | 446 (≥) | 34 | 23 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.33 | - | |||
| 159 | 439 | - | 42.3 | 121 | - | ||
| 471 | - | 33 | 33.2 | 212 | 221 | 
Heat treated : 1178°C - 1834°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com