1.2363 Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel | 1.2363 | |||
| X6CrMo4 | |||||
| X6CrMo 15-5 | |||||
| 1.2353 | |||||
| 27CrMoV6-12 | |||||
| 1.2361 | |||||
| X9CrMoV8 | |||||
| 1.2362 | |||||
| X63CrMoV5-1 | |||||
| X100CrMo5 | |||||
| X100CrMoV5-1 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| 0.95-1.05 | 0.10-0.40 | 0.40-0.80 | 0.030 | 0.030 | 4.80-5.50 | 0.90-1.20 | V 0.15-0.35 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 852 (≥) | 512 (≥) | 22 | 34 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.33 | - | |||
| 471 | 547 | - | 42.3 | 413 | - | ||
| 221 | - | 34 | 41.2 | 344 | 322 | 
Heat treated : 1285°C - 1956°C