Germany DIN X130W5 Cold working alloy tool steel and X130W5 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | X130W5 | DIN | Germany | Cold working alloy tool steel | 
| 73MoV5-2 | |||||
| 1.2414 | |||||
| 120W4 | |||||
| 1.2419 | |||||
| 105WCr6 | |||||
| 1.2436 | |||||
| X210CrW12 | |||||
| 1.2442 | |||||
| 115W8 | |||||
| 1.2453 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | W(%) | 
|---|---|---|---|---|---|---|
| 1.25-1.35 | 0.20-0.30 | 0.20-0.40 | Max 0.035 | Max 0.035 | Max 0.20 | 4.70-5.20 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 532 (≥) | 621 (≥) | 21 | 23 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.42 | - | |||
| 121 | 823 | - | 23.3 | 244 | - | ||
| 296 | - | 34 | 42.2 | 311 | 414 | 
Heat treated : 1733°C - 1177°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com