USA UNS T11346 Molybdenum series High-speed tool steel and T11346 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | T11346 | UNS | USA | Molybdenum series High-speed tool steel | 
| T11336 | |||||
| M41 | |||||
| T11341 | |||||
| M42 | |||||
| T11342 | |||||
| M43 | |||||
| T11343 | |||||
| M44 | |||||
| T11344 | |||||
| M46 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) | Co(%) | 
|---|---|---|---|---|---|---|---|---|---|
| 1.22-1.30 | 0.40-0.65 | 0.20-0.40 | ≤0.030 | ≤0.030 | 3.70-4.20 | 8.00-8.50 | 3.00-3.30 | 1.90-2.20 | 7.80-8.80 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 878 (≥) | 294 (≥) | 22 | 22 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.23 | - | |||
| 651 | 476 | - | 12.3 | 442 | - | ||
| 937 | - | 31 | 24.2 | 342 | 344 | 
Heat treated : 1435°C - 1526°C