Japan JIS SKS4 shock-resistant steel and SKS4 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | SKS4 | JIS | Japan | shock-resistant steel | 
| SK7 | |||||
| SK60 | |||||
| SKS11 | |||||
| SKS2 | |||||
| SKS21 | |||||
| SKS5 | |||||
| SKS51 | |||||
| SKS7 | |||||
| SKS81 | |||||
| SKS8 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | W(%) | 
|---|---|---|---|---|---|---|
| 0.45-0.55 | Max 0.35 | Max 0.50 | Max 0.030 | Max 0.030 | 0.50-1.00 | 0.50-1.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 451 (≥) | 498 (≥) | 14 | 12 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.14 | - | |||
| 866 | 874 | - | 12.3 | 314 | - | ||
| 523 | - | 41 | 13.2 | 342 | 142 | 
Heat treated : 1919°C - 1144°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| SKS4 | JIS | Japan | shock-resistant steel | 
| SKS41 | JIS | Japan | shock-resistant steel | 
| SKS43 | JIS | Japan | shock-resistant steel | 
| SKS44 | JIS | Japan | shock-resistant steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...